Тезис
This document specifies a method for the determination of the resistance of moulded test specimens of polypropylene and propylene-copolymers to accelerated ageing by heat in the presence of air using a forced draught oven.
The method represents an attempt to estimate the service life of parts fabricated from propylene plastics.
The stability determined by this method is not directly related to the suitability of the material for use when different environmental conditions prevail.
NOTE The specified thermal levels are considered sufficiently severe to cause failure of commercial grades of heat-stable propylene plastics within a reasonable period of time. If desired, lower temperatures can be applied to estimate the performance of propylene plastics with lower heat stabilities.
Общая информация
-
Текущий статус: ОпубликованоДата публикации: 2019-07Этап: Рассылка краткого отчета о пересмотре [90.60]
-
Версия: 2
-
Технический комитет :ISO/TC 61/SC 9ICS :83.080.20
- RSS обновления
Жизненный цикл
-
Ранее
ОтозваноISO 4577:1983
-
Сейчас
ОпубликованоISO 4577:2019
Стандарт, который пересматривается каждые 5 лет
Этап: 90.60 (Hа стадии пересмотра)-
00
Предварительная стадия
-
10
Стадия, связанная с внесением предложения
-
20
Подготовительная стадия
-
30
Стадия, связанная с подготовкой проекта комитета
-
40
Стадия, связанная с рассмотрением проекта международного стандарта
-
50
Стадия, на которой осуществляется принятие стандарта
-
60
Стадия, на которой осуществляется публикация
-
90
Стадия пересмотра
-
95
Стадия, на которой осуществляется отмена стандарта
-
00