Abstract
The method consists in ashing of a test portion in a muffle furnace at 525+25 C, treating the ash obtained with hydrochloric acid, neutralizing with ammonia solution and determing of the value using an ammonia/ammonium chloride electrolyte. Copper, tin, lead and cadmium do not interfere.
General information
-
Status: PublishedPublication date: 1986-04Stage: International Standard confirmed [90.93]
-
Edition: 1Number of pages: 3
-
Technical Committee :ISO/TC 34/SC 3ICS :67.080.01